PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric

Durable, versatile 0.9mm PVC-coated fabric for inflatable boats and marine applications.

规格

重量(g/m²) 650 g/m² (typical)
宽度(m) 1.5 m (custom)
厚度(mm) 0.9 mm
颜色 Custom
材料 PVC-coated polyester
拉伸强度(N/5cm) Warp ≥ 2500 N/5cm, Weft ≥ 2000 N/5cm
撕裂强度(N) Warp ≥ 250 N, Weft ≥ 200 N
附着力(N/5cm) ≥ 100 N/5cm
阻燃标准 Optional
发送询盘

产品详情

Pvc Inflatable Boat Fabric 0 9mm Industrial Grade Coated Fabric PVC Inflatable Boat Fabric 0.9mm

Product Introduction

Our PVC inflatable boat fabric 0.9mm is a high-performance coated fabric designed for the demanding marine environment. This material combines a polyester scrim with a robust PVC coating, offering excellent strength, flexibility, and resistance to abrasion, UV, and chemicals. It is the ideal choice for manufacturers of inflatable boats, kayaks, and other watercraft requiring reliable, long-lasting performance.

Technical Parameters

  • Weight: 650 g/m² (typical)
  • Width: 1.5 m (custom widths available)
  • Thickness: 0.9 mm
  • Color: Custom (commonly white, grey, orange, or military green)
  • Material: PVC-coated polyester fabric
  • Tensile Strength: Warp ≥ 2500 N/5cm, Weft ≥ 2000 N/5cm (typical)
  • Tear Strength: Warp ≥ 250 N, Weft ≥ 200 N (typical)
  • Adhesion Strength: ≥ 100 N/5cm (coating to fabric)
  • Flame Retardancy: Optional (meets various standards)

Parameter Analysis

  • Thickness (0.9mm): Provides a balance of flexibility and rigidity, making it easy to handle while offering sufficient puncture resistance for recreational and professional use.
  • Tensile and Tear Strength: The high tensile and tear values ensure the fabric withstands stress from water pressure, impacts, and handling.
  • Adhesion Strength: Strong adhesion between the PVC coating and the polyester base prevents delamination, even under prolonged exposure to water and sunlight.
  • Flame Retardancy: Optional treatment enhances safety in marine environments.

Application Scenarios

  • Inflatable Boats: Ideal for hulls, tubes, and air chambers.
  • Kayaks and Canoes: Lightweight yet durable for paddling crafts.
  • Rafts and Dinghies: Suitable for rescue, leisure, and commercial use.
  • Repair Patches: Used for patching and reinforcing existing inflatable products.

Installation Guide

  1. Cutting: Use sharp tools to cut the fabric to the desired shape, allowing for seam allowances.
  2. Welding: Use hot air welding or high-frequency welding equipment to join panels. Ensure surfaces are clean and dry.
  3. Sealing: Apply PVC adhesive or sealant to seams for extra watertightness.
  4. Valve Installation: Attach valves according to manufacturer instructions, ensuring airtight seals.

Usage Method

  • Inflate the boat to the recommended pressure (usually 0.25–0.3 bar for tubes).
  • Avoid over-inflation, which can stress the fabric.
  • Use on clean water surfaces to minimize abrasion.
  • Follow local regulations for safe operation.

Maintenance Advice

  • Rinse with fresh water after each use in saltwater.
  • Dry thoroughly before storage to prevent mildew.
  • Store in a cool, dry place away from direct sunlight.
  • Inspect regularly for signs of wear or damage.

Repair Tips

  • Clean the damaged area and cut a patch larger than the damaged spot.
  • Apply PVC adhesive to both surfaces, press firmly, and allow to cure.
  • For small punctures, use a repair kit with PVC patches and glue.

Procurement Advice

  • Specify your required width, color, and any special treatments (e.g., flame retardant).
  • Request samples for testing before bulk order.
  • Consider minimum order quantities and lead times.
  • Verify compliance with relevant marine standards if required.

Packaging List

  • Rolls of fabric (typically 50–100 meters per roll)
  • Protective wrapping (kraft paper or PE film)
  • Packing list and quality certificate

FAQ

Q: What is the standard width?

A: Standard width is 1.5 meters, but custom widths are available.

Q: Is this fabric suitable for saltwater use?

A: Yes, it is resistant to saltwater and UV, but rinsing with fresh water after use is recommended.

Q: Can I weld this fabric with a hot air welder?

A: Yes, hot air welding and high-frequency welding are both suitable.

Q: What colors are available?

A: We offer custom colors; common options include white, grey, orange, and military green.

Q: Does the fabric meet any fire safety standards?

A: Flame retardant options are available; please specify your required standard.

This PVC inflatable boat fabric 0.9mm is a reliable choice for manufacturers seeking quality and performance. Contact us for more details and customization options.

常见问题

PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric是什么?

PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric 是科智薄新材料生产的涂层织物产品,归属于「Coated Fabrics」分类。本页面的产品详情包含其完整规格参数。

如何获取 PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric 的报价?

请通过本页面的询盘表单发送您的需求——例如克重、门幅、颜色及预期应用——科智薄销售团队将回复您的规格所对应的价格与交期。

科智薄是否为 PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric 提供 OEM/ODM 定制?

是的。科智薄为旗下涂层织物产品提供 OEM/ODM 服务,可根据您的项目需求调整规格参数。欢迎联系我们的团队洽谈细节。

科智薄是否拥有 ISO 认证?

是的。科智薄已通过 ISO 9001 质量管理体系认证,本网站新闻栏目发布了相关公告。

PVC Inflatable Boat Fabric 0.9mm – Industrial Grade Coated Fabric 是否符合阻燃标准?

请查看本页面规格表中的「阻燃标准」一栏。如需特定防火等级证书,请在询盘中注明,科智薄将为您确认可选方案。

发送询盘

未选择任何文件

支持:PDF、DOC、DOCX、JPG、PNG、XLS、XLSX。最大5MB。

发表评论

您的邮箱地址不会被公开。 必填项已用 * 标注