跳到内容

PVC Geomembrane

High-performance flexible waterproofing membrane for environmental and civil engineering applications.

规格

重量(g/m²) Custom
宽度(m) Custom
厚度(mm) Custom
颜色 Black, blue, green, or custom
材料 PVC
拉伸强度(N/5cm) Custom (≥15 MPa)
撕裂强度(N) Custom (≥60 N/mm)
附着力(N/5cm) Custom (peel ≥30 N/50mm)
阻燃标准 Custom (optional)
发送询盘

产品详情

PVC Geomembrane

PVC geomembrane: flexible impermeable sheet for containment barriers — fish ponds, aquaculture, landfills, tailings ponds, drinking water tanks, biogas digesters, agricultural canals. Thickness 0.5–1.5 mm; 0.5–0.75 mm for ponds/agriculture, 0.75–1.5 mm reinforced for landfills and potable water. Weldability is critical for leak-free installations.

Technical Specifications

Application Thickness Standard Key property
Pond / agricultural liner 0.5 mm (20 mil) ASTM D7176 pH 2–12 resistant, UV-stabilized
Landfill liner / cover 0.75 mm (30 mil) ASTM D7176 / GRI-GM17 Chemically resistant, weldable
Potable water tank (reinforced) 1.0–1.5 mm GRI-GM17 + NSF/ANSI 61 Drinking-water certified
Biogas digester 0.75–1.5 mm reinforced Custom Gas-tight, biogas-resistant

Market Compliance & Import Considerations

Region Key standard
Europe REACH phthalates/lead; NSF/ANSI 61 if drinking-water contact; HS 5903.10.90 ≈ 8%
USA ASTM D7176 (PVC geomembrane); GRI GM15/GM34 (PVC-EIA); NSF/ANSI 61; HS 5903.10.15 = DUTY FREE

Typical Applications

  • Aquaculture & fish pond liners
  • Drinking water tanks & reservoirs
  • Landfill covers & leachate containment
  • Mining tailings ponds
  • Biogas digester covers
  • Agricultural irrigation canals

How to Select the Right Specification

Small backyard pond 0.5 mm (20 mil) — ASTM D7176, UV-stabilized
Large aquaculture reservoir 0.5–0.75 mm, thicker for continuous UV exposure
Municipal / hazardous landfill Reinforced 0.75–1.5 mm / GRI-GM17, leak-detection compatible
Drinking water storage Reinforced 1.0–1.5 mm / NSF/ANSI 61 certified
Strong solvents / hydrocarbons Switch to PVC-KEE / PVC-EIA or HDPE — consult engineer before quoting

Welding & Installation

NOTE PVC geomembrane MUST use hot-air / heat-wedge / RF / solvent welding. NOT extrusion welding. Weld overlap: 100–150 mm.

Procurement Checklist

  • Specify: tensile + tear + peel requirements, fire rating per local code, surface finish (PVDF/acrylic/matte), print ink compatibility
  • All values are industry-typical ranges — we provide third-party lab test reports with every batch
  • Import tariffs & anti-dumping change frequently — verify the latest WTO schedule before pricing
  • Contact [email protected] with your spec requirements and target market for a quick quotation

Quality Assurance and Customization

Every PVC Geomembrane is produced under ISO 9001-controlled processes and tested to ASTM D751 for tensile, tear, and adhesion performance. Typical properties include a basis weight around Custom g/m² and a PVC construction selected for stable welding and long service life. KeZHiBo offers custom widths, colors, and surface treatments—anti-fungal, anti-static, or FR-rated—with third-party inspection available on request, supporting both OEM volumes and project-specific specifications from prototype to delivery.

常见问题

PVC Geomembrane是什么?

PVC Geomembrane 是科智博新材料生产的涂层织物产品,归属于「Geomembranes」分类。本页面的产品详情包含其完整规格参数。

如何获取 PVC Geomembrane 的报价?

请通过本页面的询盘表单发送您的需求——例如克重、门幅、颜色及预期应用——科智博销售团队将回复您的规格所对应的价格与交期。

科智博是否为 PVC Geomembrane 提供 OEM/ODM 定制?

是的。科智博为旗下涂层织物产品提供 OEM/ODM 服务,可根据您的项目需求调整规格参数。欢迎联系我们的团队洽谈细节。

科智博是否拥有 ISO 认证?

是的。科智博已通过 ISO 9001 质量管理体系认证,本网站新闻栏目发布了相关公告。

PVC Geomembrane 是否符合阻燃标准?

请查看本页面规格表中的「阻燃标准」一栏。如需特定防火等级证书,请在询盘中注明,科智博将为您确认可选方案。

发送询盘

未选择任何文件

支持:PDF、DOC、DOCX、JPG、PNG、XLS、XLSX。最大5MB。

发表评论

您的邮箱地址不会被公开。 必填项已用 * 标注